Q1:

If the iron ore contains clay as an impurity, the flux added during calcination, is

A clay

B lime stone

C argillaceous iron ore

D all the above.

ANS:B - lime stone

I think caco3 calcinate into cao (quick lime) which is unstable. And cao reacts with clay to form slag.